Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0155 cm/cm
0.0155 in/in
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo..
Linear Mold Shrinkage, Transverse 0.0155 cm/cm
0.0155 in/in
STN 64 0808
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc
FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden..
Linear Mold Shrinkage, Transverse 0.0155 cm/cm
0.0155 in/in
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden..
Linear Mold Shrinkage, Transverse 0.0155 - 0.0185 cm/cm
0.0155 - 0.0185 in/in
LATI Latistat 52/7-02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Linear Mold Shrinkage, Transverse 0.0155 cm/cm
0.0155 in/in
Solvay TECHNYL® A 221 Natural FA PA66, DRY
Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv..