Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 10% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitable for automotive, engineering, electrical and consumer goods industry. With the increasing content of GF also the toughness, tensile and bending strength, modulus in tension and bending increase and the shrinkage decreases as well as the heat application increases up to 150°C. Additional drying of the material is not necessary. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Linear Mold Shrinkage 0.0195 cm/cm
0.0195 in/in
Linear Mold Shrinkage, Transverse 0.0185 cm/cm
0.0185 in/in
Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
Elongation at Break 4.0 %
4.0 %
Tensile Modulus 3.10 GPa
450 ksi
Flexural Strength 55.0 MPa
7980 psi
Flexural Modulus 2.00 GPa
290 ksi
Charpy Impact Unnotched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.100 J/cm²

@Temperature -20.0 °C
0.476 ft-lb/in²

@Temperature -4.00 °F
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Vicat Softening Point 130 °C
266 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi