Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 10% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitabl..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -20.0 °C
22.8 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 25 FRC 4 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 25 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability according to UL 94 3 at 1,6mm, glow wire at 960°C. Applic..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -20.0 °C
22.8 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre
FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre
FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -30.0 °C
22.8 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A RV200 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -30.0 °C
22.8 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S RV200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -20.0 °C
22.8 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing
Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVALEN PH 41 GF 10 Polypropylene Homopolymer, 10% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 69 GF 30 LS PP, 30% glass fibre, mod. of mech. prop., UV stability
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. UV stable. Increased strength in comparison with u..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -30.0 °C
22.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -30.0 °C
22.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced
GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. ..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -30.0 °C
22.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1fU
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -30.0 °C
22.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature -40.0 °C
22.8 ft-lb/in²

@Temperature -40.0 °F
ASTM D256
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Charpy Impact Unnotched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled
SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo..