Material Notes:
Carbon fiber added, high stiffness and conductive grade. Applications: Conductive products. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.22 %
0.22 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength 120 MPa
17400 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 175 MPa
25400 psi
ASTM D790
Flexural Modulus 13.7 GPa
1990 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Melting Point 166 °C
331 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
324 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257