Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Temperature 22.8 °C
3.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1000 - 1.00e+6 ohm-cm
1000 - 1.00e+6 ohm-cm
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 274 - 316 °C
525 - 600 °F
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Dry Time 2 - 4 hour

@Temperature 121 °C
2 - 4 hour

@Temperature 250 °F
to ensure the moisture level is less than 0.02%
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Secondary
68.9 - 138 MPa
10000 - 20000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm