Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0185 cm/cm | 0.0185 in/in | |
Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre FeaturesModified copolymer PP for injection moulding, chemically reinforced with 10% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitabl.. |
|||
Linear Mold Shrinkage, Transverse | 0.0185 cm/cm | 0.0185 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 41 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Linear Mold Shrinkage, Transverse | 0.0185 cm/cm | 0.0185 in/in | ISO 294-4 |
DSM Akulon® K230-HPV8 Impact Modified Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.0185 - 0.021 cm/cm | 0.0185 - 0.021 in/in | |
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |