Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 11 with PTFE Filler

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11 with PTFE Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 11 with PTFE Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.09 - 1.15 g/cc
0.0394 - 0.0415 lb/in³
Average value: 1.11 g/cc Grade Count:5
Linear Mold Shrinkage 0.0130 - 0.0250 cm/cm
0.0130 - 0.0250 in/in
Average value: 0.0169 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 - 48.3 MPa
5000 - 7000 psi
Average value: 40.7 MPa Grade Count:5
Elongation at Break 10.0 %
10.0 %
Average value: 10.0 % Grade Count:5
Modulus of Elasticity 1.38 - 1.72 GPa
200 - 250 ksi
Average value: 1.54 GPa Grade Count:5
Flexural Yield Strength 44.8 - 55.2 MPa
6500 - 8000 psi
Average value: 49.6 MPa Grade Count:5
Flexural Modulus 1.38 - 1.72 GPa
200 - 250 ksi
Average value: 1.59 GPa Grade Count:5
Izod Impact, Notched 0.534 - 0.747 J/cm
1.00 - 1.40 ft-lb/in
Average value: 0.651 J/cm Grade Count:5
Izod Impact, Unnotched 10.7 - 5340 J/cm
20.0 - 10000 ft-lb/in
Average value: 12.0 J/cm Grade Count:5
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 54.4 °C
120 - 130 °F
Average value: 51.1 °C Grade Count:5
Flammability, UL94 HB
HB
Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 216 - 282 °C
420 - 540 °F
Average value: 243 °C Grade Count:4
Mold Temperature 37.8 - 104 °C
100 - 220 °F
Average value: 71.7 °C Grade Count:5
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:5