Mechanical Properties Metric English Comments
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resista..
Modulus of Elasticity 1.38 GPa
200 ksi
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze
The addition of 60% bronze to the base material reduces the expansion coefficient and gives lower sliding wear.Special Properties:• Lower sliding wear than Murflor®• Good slide properties• Low s..
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio..
Modulus of Elasticity 1.38 - 1.72 GPa
200 - 250 ksi
Average value: 1.54 GPa Grade Count:5
Overview of materials for Nylon 11 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 1.38 - 2.23 GPa
200 - 323 ksi
Average value: 1.91 GPa Grade Count:4
Overview of materials for Nylon 11 with Graphite Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Total PPH 3230 Polypropylene, Blow Molding Grade
Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim..
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Total PPH 3429 Polypropylene, Injection Molding Grade
LTHA injection molding homopolymerLTHA - FINA 3429 is engineered with an LTHA additive system that gives excellent leach resistance in hot/wet environments that contain bleach and laundry detergents..
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Total PPH 3622 Polypropylene, Injection Molding Grade
General purpose injection molding and extrusion homopolymerGood Processability -- FINA 3622 is engineered for good processability in thin wall multi- cavity molds.Good Clarity -- FINA 3622 has good ..
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Total PPR 3230XZ Polypropylene, Blow Molding Grade
Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac..
Modulus of Elasticity 1.38 GPa
200 ksi
IPC TM-650 2.4.18.3
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist..
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Plaskolite West Optix® CA-1000 IG Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio..
Modulus of Elasticity 1.38 - 3.52 GPa
200 - 510 ksi
Average value: 2.13 GPa Grade Count:92
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Modulus of Elasticity 1.38 - 46.0 GPa
200 - 6670 ksi
Average value: 19.2 GPa Grade Count:16
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 1.38 - 3.45 GPa
200 - 500 ksi
Average value: 2.16 GPa Grade Count:23
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Modulus of Elasticity 1.38 - 2.96 GPa
200 - 430 ksi
Average value: 2.06 GPa Grade Count:13
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded