Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 54.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 43.3 - 54.4 °C
110 - 130 °F
ASTM D648
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 54.4 °C
120 - 130 °F
Average value: 51.1 °C Grade Count:5
Overview of materials for Nylon 11 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved