Processing Properties Metric English Comments
Processing Temperature 216 - 282 °C
420 - 540 °F
Average value: 243 °C Grade Count:4
Overview of materials for Nylon 11 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr..
Processing Temperature 216 - 282 °C
420 - 540 °F
Average value: 249 °C Grade Count:3
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Processing Temperature 216 - 266 °C
420 - 510 °F
Average value: 244 °C Grade Count:5
Overview of materials for Nylon 12, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Processing Temperature 216 - 266 °C
420 - 510 °F
Average value: 241 °C Grade Count:5
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Processing Temperature 216 - 266 °C
420 - 510 °F
Average value: 241 °C Grade Count:3
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Processing Temperature 216 °C
421 °F
Film extrusion temperature
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade
DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re..
Processing Temperature 216 °C
420 °F
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCHT Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040NCHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with improved surface ..
Processing Temperature 216 °C
420 °F
Advanced Polymer Alloys DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE features excellent so..
Processing Temperature 216 - 282 °C
420 - 540 °F
Average value: 251 °C Grade Count:3
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..