Processing Properties Metric English Comments
Mold Temperature 37.8 - 43.3 °C
100 - 110 °F
Northstar Polymers MPP-R07B Polyurethane Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-..
Mold Temperature 37.8 - 54.4 °C
100 - 130 °F
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at ..
Mold Temperature 37.8 - 93.3 °C
100 - 200 °F
RTP Company RTP 3481-1 Liquid Crystal Polymer (LCP), Carbon Fiber
Mold Temperature 37.8 - 93.3 °C
100 - 200 °F
Celanese Vandar® 4612R PBT, 7% Glass Reinforced  (Unverified Data**)
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 401 FR Polystyrene (PS), Glass Fiber - Flame Retardant - UL94
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 405 Polystyrene (PS), Glass Fiber
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Ineos Nova 2110 General Purpose Crystal Polystyrene  (discontinued **)
Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure..
Mold Temperature 37.8 - 48.9 °C
100 - 120 °F
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam
This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperat..
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company PermaStat® 1800A FR UV  Polycarbonate/Acrylic Alloy (PC/PMMA) Anti-Static - Flame Retardant - UV Stable
Anti-Static - Flame Retardant - UV StableComments:Permanently Anti-StaticESD ProtectionFlame RetardantUV StabilizedUnless otherwise specified, all data listed is for natural or black colored materia..
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 202C  Nylon 11 (PA 11) Glass Fiber 15%  (discontinued **)
Glass Fiber 15%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 201C FR  Nylon 11 (PA 11) Glass Fiber 10% - Flame Retardant  (discontinued *
Glass Fiber 10% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Ineos Nova 1600 High Heat Crystal Polystyrene
High heat resistance, Moderate flow, Good balance of strength and set-upApplications: Foam extrusion, Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant e..
Mold Temperature 37.8 - 93.3 °C
100 - 200 °F
Where aesthetics are critical its preferred to use 180-200ºF
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
Mold Temperature 37.8 °C
100 °F
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 203 C Nylon 11 (PA); Glass Fiber - 79% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Mold Temperature 37.8 - 82.2 °C
100 - 180 °F
Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products.
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Mold Temperature 37.8 - 82.2 °C
100 - 180 °F
Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products.
Diamond Polymers ASA S710
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 203C  Nylon 11 (PA 11) Glass Fiber 20%  (discontinued **)
Glass Fiber 20%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
RTP Company RTP 287C  Nylon 11 (PA 11) Carbon Fiber 40%  (discontinued **)
Carbon Fiber 40%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Ineos Nova 4210 Medium Impact Polystyrene  (discontinued **)
Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o..
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Ineos Nova 5470 High Impact Polystyrene  (discontinued **)
High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection molded specimens at 23°C and..
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Ineos Nova 6260 Super High Impact Polystyrene  (discontinued **)
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
Mold Temperature 37.8 - 60.0 °C
100 - 140 °F
RTP Company RTP 1205-70A  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 30% - 70 Shore A &am
Glass Fiber 30% - 70 Shore AComments:Glass Fiber70-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F
Ineos Nova 2581 General Purpose Crystal Polystyrene  (discontinued **)
Good blending resin, Good balance of flow, strength and heat resistanceApplications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no significant eff..
Mold Temperature 37.8 - 60.0 °C
100 - 140 °F
RTP Company RTP 1200-80A BLACK Ester-based Thermoplastic Polyurethane Elastomer  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Mold Temperature 37.8 - 60.0 °C
100 - 140 °F
RTP Company RTP 1207-65D  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 40% - 65 Shore D &am
Glass Fiber 40% - 65 Shore DComments:Glass Fiber65-D DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Mold Temperature 37.8 - 60.0 °C
100 - 140 °F
PolyOne Stat-Tech™ PP-CP1/000 HF6 Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Mold Temperature 38.0 - 79.0 °C
100 - 174 °F
Samsung Cheil Industries Starex® HF-5661H ASA, Unreinforced  (discontinued **)
Amorphous Styrene Acrylonitrile (SAN)Characteristics: High Flow: Impact, Heat and Chemical Resistance and Surface GlossApplications: Pens, TV Components, Refrigerator and Appliance ComponentsProcess..
Mold Temperature 37.8 - 107 °C
100 - 225 °F
Average value: 81.7 °C Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved