Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 48.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black
Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black
Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified
Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ASTM D648
Spartech PE4125 Reinforced High Density Polyethylene Compound
Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Unannealed; ASTM D648
Techmer ES Statiblend® 02056 BKN Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ISO 75-2/A
ExxonMobil Exxtral™ BMU130P Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ISO 75-2/A
ExxonMobil PP7043L1 Polypropylene Impact Copolymer
Product Description: An impact copolymer resin characterized by medium flow. It is suitable for molding applications like consumer products, containers and rigid packaging applications.Availability..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Aclo Accutech Polypropylene Copolymer CP0437M10L Mica Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Adell ZS-10 Nylon/Olefin Alloy
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Adell ZS-30 Nylon/Olefin Alloy
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Unannealed; ASTM D648
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 206 °C
120 - 402 °F
Average value: 104 °C Grade Count:29
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 211 °C
120 - 412 °F
Average value: 177 °C Grade Count:41
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..