3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D4894
Bulk Density 0.440 g/cc
0.0159 lb/in³
ASTM D4894
Particle Size 25 µm
25 µm
ASTM D4894
Deformation 2.0 %

@Pressure 15.00 MPa
2.0 %

@Pressure 2175 psi
ASTM D621
4.0 %

@Time 86400 sec,
Pressure 15.00 MPa
4.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
Initial; ASTM D2240
63

@Time 15.0 sec
63

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D4894
Elongation at Break 160 %
160 %
ASTM D4894
Tensile Modulus 0.217 GPa
31.5 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 88.2 µm/m-°C

@Temperature 30.0 - 100 °C
49.0 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
119 µm/m-°C

@Temperature 100 - 200 °C
66.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
144 µm/m-°C

@Temperature 200 - 300 °C
80.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
0.370 W/m-K

@Temperature 250 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
Shrinkage 1.7 %
1.7 %
ASTM D4894