Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Murtfeldt Murdopol® Nylon 12

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Cast
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Murdopol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Murdopol® Nylon 12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its fantastic ability to create firm plastic/metal connections.Special Properties:• Good shock and impact resistance• Low residual stress• Metal core surrounded by cast plastic available• Good damping and vibration behavior• Lowest moisture absorption of all polyamides• Good resistance to chemicals• Dimensionally stableInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.90 %

@Temperature 23.0 °C
0.90 %

@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 1.4 %

@Temperature 23.0 °C
1.4 %

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
DIN 53505
Tensile Strength, Yield 55.0 MPa
7980 psi
dry; ISO 527-1
55.0 MPa
7980 psi
50% RH; ISO 527-1
Elongation at Break 200 %
200 %
dry; ISO 527-1
200 %
200 %
50% RH; ISO 527-1
Modulus of Elasticity 2.00 GPa
290 ksi
dry
2.00 GPa
290 ksi
50% RH
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35
0.35
Sand Slurry 0.80
0.80
µm/km
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
120 µm/m-°C

@Temperature 23.0 - 100 °C
66.7 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
Melting Point 180 °C
356 °F
ISO 11357-1
Maximum Service Temperature, Air 120 °C

@Time 1.80e+7 sec
248 °F

@Time 5000 hour
150 °C

@Time <=86400 sec
302 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
50% RH; IEC 60093
>= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
dry; IEC 60093
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
50% RH; IEC 60093
>= 1.00e+13 ohm
>= 1.00e+13 ohm
dry; IEC 60093
Dielectric Constant 3.5

@Frequency 100 Hz
3.5

@Frequency 100 Hz
dry; IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
50% RH; IEC 60243-1
50.0 kV/mm
1270 kV/in
dry; IEC 60243-1
Dielectric Loss Index 0.038

@Frequency 100 Hz
0.038

@Frequency 100 Hz
dry; IEC 60250
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Natural