Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 120 °C @Time 1.80e+7 sec |
248 °F @Time 5000 hour |
|
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Maximum Service Temperature, Air | 120 °C @Time 1.80e+7 sec |
248 °F @Time 5000 hour |
|
Murtfeldt Murylon® A GF Nylon 66, Glass Reinforced Murylon® A’s impressive characteristics are enhanced with admixed glass fibers. This results in a clear improvement in cold flow behavior and dimensional stability, enabling higher static pressure.. |