Thermal Properties Metric English Comments
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Recommended
Nye Lubricants 227(SO) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S50Y Silicone Rubber
Yellow Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. U..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S70R Silicone Rubber
Red Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and lo..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Parker Chomerics WIN-SHIELD™ C (Cast Allycarbonate) EMI Shielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast polycarbonate. A unique feature of Parker Chomerics w..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.001" Diameter Wire, Allycarbonate EMI Shielding Window
Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lig..
Minimum Service Temperature, Air -60.0 - -30.0 °C
-76.0 - -22.0 °F
Average value: -48.2 °C Grade Count:241
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Resin Technology Group TIGA 216-EX High Performance Adhesive
Mix ratio 2 to 1 by volume.TIGA 216-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 216-EX offers a 60 minute pot life and good hardness development within..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Resin Technology Group TIGA 920H Flexible Silver Conductive
100 parts resin to 115 parts hardener.TIGA 920-H is a flexible, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications that require high flexibil..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad
Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Fujipoly Industries Sarcon® GR-n Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Momentive Performance Materials IS808 Translucent Adhesive Sealant, General Purpose Paste
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose,..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Momentive Performance Materials RTV109 Aluminum Adhesive Sealant, High Strength Paste
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Momentive Performance Materials RTV112 White Adhesive Sealant, General Purpose Pourable
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Thin-section protective ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Momentive Performance Materials RTV128 Translucent Adhesive Sealant, General Purpose Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose for bonding ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant
RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive
TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Tra-Con Tra-Bond F123 Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F123 is a fast cure, low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating sin..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Tra-Con Tra-Cast FS407 Low Viscosity High Temperature Epoxy Casting System
TRA-CAST FS407 is a low viscosity, solvent-free epoxy casting system recommended for rigid industrial laminating, electrical potting and transformer or coil embedding applications that require the e..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive
TRA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
3M 436/Silver Damping Foils
Low temperature vibration dampingInformation provided by 3M
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
3M 435/Silver Damping Foils
Low temperature vibration dampingInformation provided by 3M
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
AlphaGary Evoprene™ 3273 Standard SBS Thermoplastic Elastomer Compound
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st..
Minimum Service Temperature, Air -60.0 - -40.0 °C
-76.0 - -40.0 °F
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Resinlab® TL5090 Anaerobic Threadlocking Compound
The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a ..
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Minimum Service Temperature, Air -60.0 - -50.0 °C
-76.0 - -58.0 °F
AlphaGary Evoprene™ GC 5691 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
Minimum Service Temperature, Air -60.0 - -50.0 °C
-76.0 - -58.0 °F
AlphaGary Evoprene™ GC 5696 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
Copyright © lookpolymers.com All Rights Reserved