Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.00 GPa | 290 ksi | dry |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 2.00 GPa @Thickness 4.00 mm |
290 ksi @Thickness 0.157 in |
10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ASTM D882-02 |
NeXolve LaRC™-CP1 Polyimide Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 1850-8197 PBT, lubricant modified, easy flowing, demolding aid Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ISO 527 |
GEHR Plastics POM-ELS Acetal, Electrically Conductive Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Modulus of Elasticity | 2.00 GPa @Temperature -40.0 °C |
290 ksi @Temperature -40.0 °F |
ASTM D638 |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 18MB090 OPP Film Product Description: Biaxially oriented polypropylene film metallizable on one side, with a slip controlled broad seal range surface on the other side. Once metalized, film designed to be used in la.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB080 OPP Film Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 21MB777 OPP Film Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 25MB400 OPP Film Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 30MB400 OPP Film Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 30MB668 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 35MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 40MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 52MBR666 OPP Film Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 35LL400 OPP Film Product Description: A one-side treated, transparent coextruded OPP film. The film is slip controlled for optimal performance on reel-fed labeling machines.Availability: Africa & Middle East, Asia .. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL539 OPP Film Product Description: A clear, two-side coated, polypropylene label face stock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 57LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ISO 178 |
Addiplast Addilene J 470 ST14 Polypropylene Copolymer Soft touchInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.00 GPa | 290 ksi | ISO 178 |
Addiplast Addilene PMD 50306 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |