Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Recommended |
Nye Lubricants 822S-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Recommended |
Nye Lubricants 855B (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Recommended |
Nye Lubricants UniFlor 8990 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering S65T Silicone Rubber Translucent Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United Sta.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Precision Polymer Engineering S75R Silicone Rubber Oil Resistant, Red Silicone Rubber, 65-75 °IRHD. Diesel Liner Ring Grade. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applic.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering S80A Silicone Rubber Blue Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Fe.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.002" Diameter Wire, Allycarbonate EMI Shielding Window Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lig.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Resin Technology Group TIGA 216-EX High Performance Adhesive Mix ratio 2 to 1 by volume.TIGA 216-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 216-EX offers a 60 minute pot life and good hardness development within.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Continuous useful temperature. |
Momentive Performance Materials IS808 Translucent Adhesive Sealant, General Purpose Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose,.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Continuous useful temperature. |
Momentive Performance Materials RTV103 Black Adhesive Sealant, High Strength Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Continuous useful temperature. |
Momentive Performance Materials RTV160 White Adhesive Sealant, Non-Corrosive Pourable One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive prote.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Continuous useful temperature. |
Momentive Performance Materials RTV167 Gray Adhesive Sealant, Non-Corrosive High Strength One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Highest strength ad.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Continuous useful temperature. |
Momentive Performance Materials RTV6803 Black Adhesive Sealant, Industrial Plastic Adhesive One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Primerless adhesion to many .. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Tra-Con Tra-Bond 2170 Flexible Plastic Bonder TRA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermoplas.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows .. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Tra-Con Tra-Bond F123HV Color Keyed Thixotropic Epoxy Adhesive TRA-BOND F123 HV is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Tra-Con Tra-Bond 2104 Rigid Epoxy Staking Compound TRA-BOND 2104 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Intermittent |
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system .. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Atom Adhesives AA-BOND F253 Epoxy Adhesive AA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status.Appearance: Unmixed-Light Yellow; Mixed – Greenish.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
AlphaGary Evoprene™ 057 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Minimum Service Temperature, Air | -60.0 - -50.0 °C | -76.0 - -58.0 °F | |
AlphaGary Evoprene™ GC 5651 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |
Atom Adhesives AA-BOND F131 Epoxy Adhesive AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical .. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Standard Quality, All Colors |
BIW ASTM Class 2D3 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |
|||
Minimum Service Temperature, Air | -60.0 - -50.0 °C | -76.0 - -58.0 °F | |
AlphaGary Evoprene™ GC 5677 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Minimum Service Temperature, Air | -60.0 - -50.0 °C | -76.0 - -58.0 °F | |
AlphaGary Evoprene™ GC 5683 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Minimum Service Temperature, Air | -60.0 - -50.0 °C | -76.0 - -58.0 °F | |
AlphaGary Evoprene™ GC 640 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Standard Quality, All Colors |
BIW ASTM Class 2D4 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |