Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
|
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 150 °C |
55.6 µin/in-°F @Temperature 302 °F |
|
Murtfeldt Murinit® SP Polyphenylene Sulfide Thanks to the low fiber content and integrated solid lubricant, Murinit® SP offers an excellent combination of good slide and wear behavior, high strength, and dimensional stability – even at high.. |
|||
CTE, linear | 100 - 115 µm/m-°C @Temperature 25.0 - 200 °C |
55.6 - 63.9 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
CTE, linear | 100 µm/m-°C @Temperature >=143 °C |
55.6 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
CTE, linear | 100 µm/m-°C @Temperature >=143 °C |
55.6 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
CTE, linear | 100 µm/m-°C @Temperature >=162 °C |
55.6 µin/in-°F @Temperature >=324 °F |
Average above Tg; ISO 11359 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
CTE, linear | 100 µm/m-°C @Temperature >=55.0 °C |
55.6 µin/in-°F @Temperature >=131 °F |
above Tg |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
CTE, linear | 100 µm/m-°C @Temperature 250 °C |
55.6 µin/in-°F @Temperature 482 °F |
|
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |