Polymer Property : CTE, linear = 55.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murdopol® Nylon 12
Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f..
CTE, linear 100 µm/m-°C

@Temperature 150 °C
55.6 µin/in-°F

@Temperature 302 °F
Murtfeldt Murinit® SP Polyphenylene Sulfide
Thanks to the low fiber content and integrated solid lubricant, Murinit® SP offers an excellent combination of good slide and wear behavior, high strength, and dimensional stability – even at high..
CTE, linear 100 - 115 µm/m-°C

@Temperature 25.0 - 200 °C
55.6 - 63.9 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® B-60 PTFE, 60% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
CTE, linear 100 µm/m-°C

@Temperature >=143 °C
55.6 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
CTE, linear 100 µm/m-°C

@Temperature >=143 °C
55.6 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
CTE, linear 100 µm/m-°C

@Temperature >=162 °C
55.6 µin/in-°F

@Temperature >=324 °F
Average above Tg; ISO 11359
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
CTE, linear 100 µm/m-°C

@Temperature >=55.0 °C
55.6 µin/in-°F

@Temperature >=131 °F
above Tg
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
CTE, linear 100 µm/m-°C

@Temperature 250 °C
55.6 µin/in-°F

@Temperature 482 °F
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..