Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 180 °C | 356 °F | ISO 11357-1 |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Melting Point | 180 °C | 356 °F | ISO 11357-1 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Melting Point | 180 °C | 356 °F | |
Oceanchem Group Tetrabromobisphenol A (TBBA) Cas No.: 79-94-7Main use for epoxy resin, polycarbonate polyester, phenol resin, polyurethane etc. It is also used for polystyrene, ABS, AS, unsaturated polyester as flame-retardant-addative.Packin.. |
|||
Melting Point | 180 °C | 356 °F | |
Omnia Plastica PVDF Kynar PVDF is a relatively new fluoropolymer. Like the other fluoropolymers, its best feature is its chemical resistance. The mechanical features of PVDF are notably higher than PTFE and it does not suffe.. |
|||
Melting Point | 180 °C | 356 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Melting Point | 180 °C | 356 °F | |
Reliance Industries METABOLIX PHB Information provided by Reliance Industries |
|||
Melting Point | 180 °C | 356 °F | |
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Lowest Modulus, Nominal Shore D/15s 35. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Melting Point | 180 - 190 °C | 356 - 374 °F | Huntsman/TMA |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melting Point | 180 - 190 °C | 356 - 374 °F | ISO 3146-C |
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Melting Point | >= 180 °C | >= 356 °F | ISO 3146-C |
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Melting Point | >= 180 °C | >= 356 °F | ISO 3146-C |
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Melting Point | 180 °C | 356 °F | Peak |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 180 - 190 °C | 356 - 374 °F | MQSA 114 |
Lubrizol Advanced Materials Pearlthane® Maxi 12T85E Thermoplastic Polyurethane Elastomer PEARLTHANE® MAXI 12T85E is a polyester based TPU, supplied in form of transparent, colorless pellets, featuring medium hardness, good mechanical properties and outstanding abrasion resistance. Th.. |
|||
Melting Point | 180 - 192 °C | 356 - 378 °F | Huntsman/TMA |
Huntsman IROGRAN® A 89 E 4372 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melting Point | 180 - 200 °C | 356 - 392 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |
|||
Melting Point | 180 - 184 °C | 356 - 363 °F | |
Suqian Unitechem Light Stabilizer 201 Product Name: Hydroxyethyl Piperidinol (HS-201)Chemical Name: 1-(2'hydroxyethyl)-2,2,6,6-Tetramethyl-4-piperidinolCAS NO.: 52722-86-8Molecular Formula: C11H23NO2Application: Tetramethyl piperidinol .. |
|||
Melting Point | 180 °C | 356 °F | |
Solvay RHODAPHOSE® DIPHENYL PHOSPHINO FERROCENE Phosphorus Derivative Identification: 1,1’-BIS-(DIPHENYLPHOSPHINO) FERROCENE (DPPF)CAS: 12150 – 46 – 8Available in: Asia Pacific, Europe, Latin America and North America Applications: DPPF (1,1’-Bis(d.. |
|||
Melting Point | 180 °C | 356 °F | By DSC |
Toyobo PELPRENE™ P40BU Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Melting Point | 180 °C | 356 °F | DSC |
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, .. |
|||
Melting Point | 180 °C | 356 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® XG5858 TPC-ET Injection Molding |
|||
Melting Point | 180 °C | 356 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® XG6029 TPC-ET Extrusion Grade |
|||
Melting Point | 180 - 190 °C | 356 - 374 °F | DSC |
EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 180 °C | 356 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Melting Point | <= 180 °C | <= 356 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 01418 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 01418 is an excellent sealing materi.. |
|||
Melting Point | 180 °C | 356 °F | ISO 11357 |
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Melting Point | 180 °C | 356 °F | ASTM D3418 |
Ashley Polymers Ashlene® 925-20PF Nylon 12, PTFE Lubricated 20% filled PTFE lubricated, Nylon 12.Data provided by the manufacturer |
|||
Melting Point | 180 °C | 356 °F | By DSC |
Toyobo PELPRENE™ P40B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melting Point | 180 °C | 356 °F | ISO 11357 |
Arkema Group Rilsamid® PA 12 AMNO MED Nylon 12 Rilsamid® AMNO MED is a thermoplastic polyamide 12. This grade dedicated to injection offers the highest quality and it is specifically designed to meet the stringent requirements of the medical ap.. |
|||
Melting Point | 180 °C | 356 °F | ASTM D2117 |
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5302FR is a non-halogen, flame retardant grade.Information provided by Samyang. |