Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LUPOL GP3102 PP+MF10%, High Impact

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced, Impact Modified
Manufacturer LG Chemical
Trade Name LUPOL
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LG Chemical LUPOL GP3102 PP+MF10%, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Maximum Moisture Content 0.010
0.010
Injection Molding
Linear Mold Shrinkage, Flow 0.0090 - 0.014 cm/cm
<br>@Thickness 3.20 mm
0.0090 - 0.014 in/in
<br>@Thickness 0.126 in
ASTM D955
Melt Flow 10 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
10 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.4 MPa
<br>@Thickness 3.20 mm
4120 psi
<br>@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 80 %
<br>@Thickness 3.20 mm
80 %
<br>@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 35.3 MPa
<br>@Thickness 6.40 mm
5120 psi
<br>@Thickness 0.252 in
1.3mm/min; ASTM D790
Flexural Modulus 1.57 GPa
<br>@Thickness 6.40 mm
228 ksi
<br>@Thickness 0.252 in
1.3mm/min; ASTM D790
Izod Impact, Notched >= 0.883 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
>= 1.65 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
<br>@Thickness 3.20 mm
266 °F
<br>@Thickness 0.126 in
Unannealed; ASTM D648
UL RTI, Electrical 65.0 °C
<br>@Thickness >=1.50 mm
149 °F
<br>@Thickness >=0.0591 in
UL RTI, Mechanical with Impact 65.0 °C
<br>@Thickness >=1.50 mm
149 °F
<br>@Thickness >=0.0591 in
UL RTI, Mechanical without Impact 65.0 °C
<br>@Thickness >=1.50 mm
149 °F
<br>@Thickness >=0.0591 in
Flammability, UL94 HB
<br>@Thickness >=1.50 mm
HB
<br>@Thickness >=0.0591 in
Processing Properties Metric English Comments
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
Middle Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
Nozzle Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
Melt Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Injection Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
Back Pressure 29.4 - 58.8 MPa
4260 - 8530 psi
Injection Molding
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding