Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
PolyMirae Moplen EP540S Injection Molding Grade Polypropylene Moplen EP540S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540S is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
PolyMirae Moplen EP640R Injection Molding Grade Polypropylene Moplen EP640R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640R is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
PolyMirae Moplen EP640S Injection Molding Grade Polypropylene Moplen EP640S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640S is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
PolyMirae Moplen HF600N Injection Molding Grade Polypropylene Moplen HF600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HF600N is a homopolymer with improved productivity and lower energy.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
PolyMirae Moplen HP602N Injection Molding Grade Polypropylene Moplen HP602N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP602N is a homopolymer particularly suitable for injection molding.. |
|||
Flexural Modulus | 1.57 - 11.0 GPa | 228 - 1600 ksi | Average value: 5.37 GPa Grade Count:127 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 1.57 - 8.62 GPa | 228 - 1250 ksi | Average value: 4.38 GPa Grade Count:83 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
Hyosung Topilene F603 PP F603 Film Grade HomopolymerApplications: CPPCharacteristics:ProcessabilityTransparencystiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.57 GPa @Thickness 6.40 mm |
228 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333HI4 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
Kostat BK-STAT BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the .. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D760 |
LG Chemical SEETEC H7511 Polypropylene, Homopolymer Features: Seetec H7511 is designed for the extrusion of staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and UV stability. SEETEC H7511 mee.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D760 |
LG Chemical SEETEC H7525 Polypropylene, Homopolymer Features: Seetec H7525 is designed for the extrusion of staple fibers. This grade is characterized by Medium MWD and good thermobonding, with anti-gas fading stabilization. SEETEC H7525 meets the FD.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D760 |
LG Chemical SEETEC H7600 Polypropylene, Homopolymer Features: Seetec H7600 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by medium MWD and good heat stability. SEETEC H7600 meets the FDA requ.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D760 |
LG Chemical SEETEC H7630 Polypropylene, Homopolymer Features: Seetec H7630 is designed for the extrusion of continuous filament (CF) & bulk continuous filament (BCF) fibers and staple fibers. This grade is characterized by medium MWD, with anti-gas f.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
Gromax CCP PBT 1100-220S Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
Hyosung Topilene J800 PP J800 Injection General HomopolymerApplications: General injectionCharacteristics:FlowabilityStiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
Hyosung Topilene J800R PP J800R Injection Special Purpose GradeApplications:Electric home applianceHousewares applianceCharacteristics:Long-term heat resistanceInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.57 GPa @Thickness 6.40 mm |
228 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 5 mm/min; ISO 178 |
Gromax BTE65-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 5 mm/min; ISO 178 |
Gromax BTE70-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | |
Shinil Chemical SHINSTAT PP Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | ASTM D790 |
Teknor Apex Synres® SR 4336 Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Flexural Modulus | 1.57 GPa | 228 ksi | |
Zylog Hipolyene® GM BP 11 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.57 GPa @Thickness 6.40 mm |
228 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |