Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55173R062 0.0622" (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55173R062 0.0622" (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 74.9 microns
2.95 mil
Interleave
478 microns
18.8 mil
Substrate; Arlon SQA-TMS-003
551 microns
21.7 mil
Side 1; Arlon SQA-TMS-003
551 microns
21.7 mil
Side 2; Arlon SQA-TMS-003
1580 microns
62.2 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Silicone Property; ASTM D2240
75
75
Product Property; ASTM D2240
Tensile Strength 8.07 MPa
1170 psi
Silicone Property; ASTM D412
Elongation at Break 682 %
682 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.0 °C
60.0 Month

@Temperature 73.4 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally White
Substrate
Red
Total Product Weight (g/m2) 2047
Arlon SQA-TMS-025