Polymer Property : Flexural Yield Strength = 5120 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 35.3 MPa

@Thickness 6.40 mm
5120 psi

@Thickness 0.252 in
1.3mm/min; ASTM D790
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow
Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica..
Flexural Yield Strength 35.3 MPa

@Thickness 6.40 mm
5120 psi

@Thickness 0.252 in
1.3mm/min; ASTM D790
LG Chemical LUPOL GP3102 PP+MF10%, High Impact
Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical