Solvay RHODAPEX® ESB-70/A2 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPEX® ESB-70/A2 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: SODIUM ALKYL ETHER SULFATECAS: 68585-34-2 Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX ESB-70/A2 is a high foaming workhorse surfactant for alkali cleaners, mild dish wash, laundry liquids, shampoos, bath products, liquid soaps and related cosmetic products.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
pH 7.0 - 9.0
7.0 - 9.0
4% Solution; RP-17601
Optical Properties Metric English Comments
Transmission, Visible >= 95 %

@Wavelength 440 nm
>= 95 %

@Wavelength 440 nm
25% Active 80:20 H2O/IPA; RP-17605
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Viscous Paste
RP-17620
Color Practically colorless
Composition Active
69-71%, MW 382, RP-17501
Free Oil
<3%, RP-17303
Sodium Chloride
<0.5%, RP-17504
Sodium Sulfate
<2%, RP-17503
Odor Characteristic
Setting point 7°C
Users viewing this material also viewed the following: