Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 - 120 °C | 149 - 248 °F | Average value: 90.7 °C Grade Count:11 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness 0.038 inches. |
LyondellBasell Pro-fax 6331W Polypropylene Homopolymer, Antistat Key Features: antistatic polypropylene homopolymer resin, FDA acceptable, resists dust pickup, low odor transferApplications: containers, closures, hospital and institutional ware, toysMeets FDA req.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness of 0.039 inches. |
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Key Features: high flow, compatible with hindered amine light stabilizers, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpageAppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.700 mm |
149 °F @Thickness >=0.0276 in |
|
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL LW4302 PP+GF/MF30% Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl PX1115 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1115 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL PX1115 is V1 at 1.2 mm according UL94 and halogen free according VDE/DIN 472 part 815.Th.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006S Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006S is a 20% talc filled homopolymer polypropylene compound formulated with an internal mold release. Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006S Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006S is a 20% talc filled homopolymer polypropylene compound formulated with an internal mold release. Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® BG50XFI PA6 (Dry) Description: Ultramid BG50XFI is an impact modified, injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® BU50I PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
UL RTI, Mechanical with Impact | 65.0 - 120 °C | 149 - 248 °F | Average value: 76.0 °C Grade Count:9 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |