Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ASTM D955 |
PolyOne Nymax™ 1280 A HS Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ASTM D955 |
PolyOne Nymax™ 623 HS Black 13 1 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.014 cm/cm | 0.0080 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.014 cm/cm | 0.0080 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 5035D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | |
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | |
LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific) LNP* PFP36 is a compound based on Nylon 6 containing Glass Fiber and PTFE/Silicone. Characteristics are Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific) PPE+PA Unfilled GTX |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ASTM D955 |
Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content Features: Heat StabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | DIS 294-4 |
Wellman Wellamid® FRGS25-66-NBK3 Nylon 66, 25% Glass Sphere Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 4.00 mm |
0.011 - 0.014 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | on Tensile Bar; E2P method |
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | ASTM D955 |
Clariant Renol PPSP0017 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |