Polymer Property : Melt Temperature = 230 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 220 - 230 °C
428 - 446 °F
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin
Film Properties.Data provided by the manufacturer.
Melt Temperature 190 - 230 °C
374 - 446 °F
C 9021 GV1/30 POM, 30% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 26 % glass fibersInformation provided by Celanese
Melt Temperature 200 - 230 °C
392 - 446 °F
Start Point: 220°C
Kingfa FW-650 Flame Retardant ABS
Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Melt Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical HIPS 410AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection Molding
LG Chemical KEYFLEX BT 1047D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL HI5204H PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Melt Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Melt Temperature 200 - 230 °C
392 - 446 °F
Extrusion
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren..
Melt Temperature 200 - 230 °C
392 - 446 °F
Extrusion
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet..
Melt Temperature 200 - 230 °C
392 - 446 °F
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Melt Temperature 180 - 230 °C
356 - 446 °F
Extrusion
Stellarchem AB-860LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem AB870LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem LP-855 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 180 - 230 °C
356 - 446 °F
Extrusion
Styrolution Styrolux HS 70 SBC
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection Temp
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem MP-860Q TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 200 - 230 °C
392 - 446 °F
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes
BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured..
Melt Temperature 210 - 230 °C
410 - 446 °F
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o..
Melt Temperature 210 - 230 °C
410 - 446 °F
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according..
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Teknor Apex Uniprene® UN-7010-87NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Teknor Apex Uniprene® UN-7010-55NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection-molding
BASF Ultraform® N2320 006 POM
Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection-molding
BASF Ultraform® S1320 003 POM
Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat..
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection molding
BASF Ultraform® N2320 0035 POM
Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF
Melt Temperature 190 - 230 °C
374 - 446 °F
C 9021 GV1/10 POM, 10% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 10 % glass fibersInformation provided by Celanese
Melt Temperature 190 - 230 °C
374 - 446 °F
M10AE POM  (Unverified Data**)
POM copolymerHigh melt strengthInformation provided by Celanese