Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.014 cm/cm | 0.0080 - 0.014 in/in | ASTM D955 |
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 5035D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5204B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latimass 66-04 D009 PBT Specific density compound based on Polybutylene Terephthalate (PBT). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific) LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics ULTEM SILTEM-STM1500 PEI (Europe-Africa-Middle East) SILTEM STM1500 is a flexible siloxane-polyetherimide copolymer for cable and wire coatings. RoHS compliant. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF PK003ER PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Mineral, Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.014 cm/cm @Thickness 3.20 mm |
0.013 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ASTM D955 |
Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content Features: Heat StabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6 Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66 Description: Glass Fiber Reinforced, Toughened, Weatherable Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT1699-WBK1 13% Glass Fiber Reinforced, Weatherable Black Nylon 66 Description: Glass Fiber Reinforced, Weatherable Black Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | on Tensile Bar; E2P method |
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.014 cm/cm @Time 86400 sec |
0.012 - 0.014 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |