Material Notes:
AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural, thin wall applications.Commercially available only to European based customers.Information provided by Azdel.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Laminate; ISO 2577
1.14 g/cc
1.14 g/cc
Molded plaque; ISO 2577
Filler Content 30 %
30 %
AZDEL Test
Thickness 3900 microns
154 mil
AZDEL Test
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
320 x 320 mm flat plaque; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527/4
Elongation at Break 2.6 %
2.6 %
ISO 527/4
Tensile Modulus 4.30 GPa
624 ksi
ISO 527/4
Flexural Strength 115 MPa
16700 psi
ISO 178
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179/2fn
Impact 4500

@Thickness 4.00 mm
4500

@Thickness 0.157 in
Multi-axial in Newtons, at max. force; ISO 6603-2
Impact Test 15.0 J

@Thickness 4.00 mm
11.1 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
40.0 J

@Thickness 4.00 mm
29.5 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature 0.000 - 120 °C
20.0 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
48.0 µm/m-°C

@Temperature -30.0 - 0.000 °C
26.7 µin/in-°F

@Temperature -22.0 - 32.0 °F
100 x 15 x 3 mm sample; AZDEL Test
Melting Point 115 °C
239 °F
Recrystallizing temperature; ISO 3146
166 °C
331 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F
ISO 75/2a
Processing Properties Metric English Comments
Processing Temperature 205 - 220 °C
401 - 428 °F
Surface temperature
Mold Temperature 30.0 - 90.0 °C
86.0 - 194 °F
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity