Polymer Property : Specific Gravity = 1.11 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
23/23°C; ASTM D792
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.11 g/cc
1.11 g/cc
23/23°C; ASTM D792
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.11 g/cc
1.11 g/cc
23/23°C; ASTM D792
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D 792
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Specific Gravity 1.11 g/cc
1.11 g/cc
LG Chemical EM600A Impact modifier for Engineering Plastics
LG Chem impact modifiers for Engineering Plastics are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modifiers - Buta..
Specific Gravity 1.11 g/cc
1.11 g/cc
LG Chemical PA910 Processing aid
Description: General purposeApplication: Sheet, window profile, pipe etcInformation provided by LG Chemical
Specific Gravity 1.11 g/cc
1.11 g/cc
Kuraray Genestarâ„¢ N1001A-M41 Nylon
Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel
Specific Gravity 1.11 g/cc
1.11 g/cc
ISO 2781
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX9406 PPE+PS
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D 792
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Spartech SolarKote® /ABS Weatherable Sheet
Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech.
Specific Gravity 1.11 g/cc
1.11 g/cc
Shin-Etsu Silicones LIMSâ„¢ KE2090-30AB Elastomer
KE-2090-30 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Specific Gravity 1.11 g/cc
1.11 g/cc
23°C; ASTM D792
Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PVX0800 PPE
NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications.
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Teknor Apex Telcar® TL-1686D Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Teknor Apex Telcar® TL-1686D1 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane
Type: Estane® ALR E68D-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
A. Schulman POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE
DescriptionPOLYBLAK® Black 4692 is a premium black color concentrate containing 35% carbon black based in LLDPE. This carbon black masterbatch is designed to provide smooth extruded surfaces and e..
Specific Gravity 1.11 g/cc
1.11 g/cc
mixed, uncured
Atom Adhesives AA-BOND FDA8 Epoxy Adhesive
AA-BOND FDA8 EPOXY ADHESIVE is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and ..
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ Metallic Grey 80330/2
DescriptionPOLYBATCH® Metallic Grey 80330/2 is a metallic grey color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH..
Specific Gravity 1.11 g/cc
1.11 g/cc
Part A
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..