Polymer Property : Processing Temperature = 428 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 170 - 220 °C
338 - 428 °F
ExxonMobil Santoprene® 60ANS200 Thermoplastic Elastomer  (discontinued **)
A soft, translucent thermoplastic elastomer (TPE) with a relative haze of 85 to 90%. This material is shear-dependent and can be processed on conventional thermoplastics equipment for injection mold..
Processing Temperature 170 - 220 °C
338 - 428 °F
Average value: 194 °C Grade Count:5
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K HTP7272/34 Super Soft Natural TPE
Natural super soft compoundComfortable hapticDry surfaceLow tackinessEasy processabilityTypical Applications: HandlesBaitsToysProtectorsMaterial Advantages: Good UV resistanceTactile surface (soft t..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TC0ADZ SEBS Black High Performance TPE
High performance SEBS compoundAdhesion to polyolefinsExcellent mechanical propertiesTypical Applications: Automotive Indoor:Anti-slip matsSoft touch for thumb wheelAir guideAir ductsSoft Touch:Trace..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TC4AAE Natural Sealing TPE
Natural compound for sealing applicationsSeals under static and dynamic loadTypical Applications: Applications in automotive and electric industries with high requirements to compression set (e.g. s..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TC9AAD SEBS Natural High Performance TPE
High performance SEBS compoundEasy to color adhesion to polyolefinsExcellent mechanical propertiesTypical Applications: Automotive Indoor:Anti-slip matsSoft touch for thumb wheelSoft Touch:TracerPus..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TF7AAE Natural TPE
Natural compound with BgVV/FDA complianceExcellent mechanical propertiesEasy to colorTypical Applications: Esthetic and functional packaging elementsCosmetics and wellness productsParts with food co..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TP5HPZ SEBS Black High Performance TPE
High performance SEBS compound, particularly for automotive exterior applicationsTypical Applications: Automotive Exterior: Application with high requirements to UV and weathering resistanceRoof tri..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TP8HLZ Exterior Automotive Sealing TPE
Black compound for exterior automotive sealing applicationsExcellent sealing performanceTypical Applications: Headlamp sealsAir drag sealingMaterial Advantages: Good compression setHigh resistance t..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TC3AAZ Black Sealing TPE
Natural compound for sealing applicationsSeals under static and dynamic loadTypical Applications: Applications in automotive and electric industries with high requirements to compression set (e.g. s..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TF3AAE Natural TPE
Natural compound with BgVV/FDA complianceExcellent mechanical propertiesEasy to colorTypical Applications: Esthetic and functional packaging elementsCosmetics and wellness productsParts with food co..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TF5AAA Natural TPE
Natural compound with BgVV/FDA complianceExcellent mechanical propertiesEasy to colorTypical Applications: Esthetic and functional packaging elementsCosmetics and wellness productsParts with food co..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TP5HKZ Exterior Automotive Sealing TPE
Black compound for exterior automotive sealing applicationsExcellent sealing performanceTypical Applications: Headlamp sealsAir drag sealingMaterial Advantages: Good compression setHigh resistance t..
Processing Temperature 200 - 220 °C
392 - 428 °F
Metering Temperature, Extrusion
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Processing Temperature 200 - 220 °C
392 - 428 °F
Metering Temperature, Extrusion
Stellarchem DIOSHY® GP-935-UB2 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Processing Temperature 200 - 220 °C
392 - 428 °F
Metering Temperature, Extrusion
Stellarchem GP-965B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Processing Temperature 190 - 220 °C
374 - 428 °F
Wanhua Chemical Wanthane® WHT-1180H Super Hard Polyester Based TPU
Low mold shrinkage, good impact resistance, perfect transparency, good mold release, fatigue resistance, chemical & hydrolytic resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 190 - 220 °C
374 - 428 °F
Wanhua Chemical Wanthane® WHT-8280H Super Hard Polyether-Based TPU
Low mold shrinkage, good impact resistance, perfect transparency, good mold release, fatigue resistance, chemical & hydrolytic resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 180 - 220 °C
356 - 428 °F
Total HDPE 56020 S High Density Polyethylene - Blow Molding
HDPE 56020 S is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack Resi..
Processing Temperature 180 - 220 °C
356 - 428 °F
Extrusion Temp
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film
LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o..
Processing Temperature 190 - 220 °C
374 - 428 °F
Extrusion Range
Arkema Group Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 3533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Processing Temperature 160 - 220 °C
320 - 428 °F
Extrusion
BASF Elastollan 1185 A W TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
BASF Elastollan S 50 A SPF TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
BASF Elastollan S 70 AWH TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Processing Temperature 205 - 220 °C
401 - 428 °F
Surface temperature
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
BASF Elastollan 890 AN TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Processing Temperature 170 - 220 °C
338 - 428 °F
PolyChem Alloy 5005 Talc Nucleator
Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weig..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TF8GMA Thermoplastic Elastomer, Conforming to FDA, adhesion to SAN, ASA, PMMA  
Material Advantages:Excellent adhesion on 2 component molding (dependent on geometry and processing)Easy to color Conforming to FDA and EN71/3High resilienceGood flow characteristicsService temperat..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TC4FRZ Thermoplastic Elastomer, Flame retardant  (Unverified Data**)
Typical Markets / Application Sectors:Electrics & ElectronicsApplication Examples:Injection molding parts for electric equipmentElectric plugsElectric grommetsSwitchboxesCable distributorsMaterial A..
Processing Temperature 180 - 220 °C
356 - 428 °F
Kraiburg TPE THERMOLAST® K TC5AAF Natural Sealing TPE
Natural compound for sealing applicationsSeals under static and dynamic loadTypical Applications: Applications in automotive and electric industries with high requirements to compression set (e.g. s..