Polymer Property : Impact Test = 11.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 15.0 J

@Temperature -18.0 °C
11.1 ft-lb

@Temperature -0.400 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
Ineos ABS Lustran® 256 Extrusion Blending Grade
Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi..
Impact Test 15.0 J

@Temperature -20.0 °C
11.1 ft-lb

@Temperature -4.00 °F
Total Penetration Energy; ISO 6603-2
Borealis Bormod™ BF970MO Polypropylene for Injection Molding
Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o..
Impact Test 15.0 J

@Temperature -30.0 °C
11.1 ft-lb

@Temperature -22.0 °F
ASTM D3763
Diamond Polymers Centrex® 835 Sheet Extrusion Grade
Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex ..
Impact Test 15.0 J

@Thickness 4.00 mm
11.1 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Impact Test 15.0 J

@Thickness 4.00 mm
11.1 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Impact Test 15.0 J

@Thickness 4.00 mm
11.1 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..