Polymer Property : Tensile Modulus = 624 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.30 GPa
624 ksi
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Tensile Modulus 4.30 GPa
624 ksi
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder
FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS
High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP FARADEX DX92079 PC (Europe-Africa-Middle East)
LNP* Faradex* DX92079 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Bead, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Mold Release...
Tensile Modulus 4.30 GPa
624 ksi
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527
Victrex® HT™ P22 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min
Polimeri Europa KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber  (discontinued **)
Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 10% glass fibres, high stiffness, very good dimensional stability. Vicat/B50 = 135°C Main application field..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527-1/-2
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls
PA6, molding grade, micro glass balls, good heat-ageing resistance
Tensile Modulus 4.30 GPa
624 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RBG16I PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RBG16I is a compound based on Nylon 66 resin containing Glass Bead, Graphite. Added features of this material include: High Impact.
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East)
LNP* STAT-KON* PD000 is a compound based on PA 6 resin containing Carbon Powder. Added features include: Electrically Conductive.
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X4870HH PC+PET
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer..
Tensile Modulus 4.30 GPa
624 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E..
Tensile Modulus 4.30 GPa
624 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp RB004 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RB004 is a compound based on PA 66 resin containing Glass Beads.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 4.30 GPa
624 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Tensile Modulus 4.30 GPa
624 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527-1/-2
Unitika M1030DH PA6, Dry
Nano composite nylonInformation provided by Unitika Ltd.
Tensile Modulus 4.30 GPa
624 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 4.30 GPa
624 ksi
50mm/min; ISO 527-1
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527-1/-2
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Tensile Modulus 4.30 GPa
624 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BK-30 PA6-GB30
Information provided by EMS Grivory
Tensile Modulus 4.30 GPa
624 ksi
ASTM D638
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Tensile Modulus 4.30 GPa

@Temperature 80.0 °C
624 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527/4
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Tensile Modulus 4.30 GPa
624 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG