Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 166 °C | 331 °F | ASTM D3418 |
Celanese Celcon® GC25A POM, 25% Glass Reinforced
(Unverified Data**) Celcon® acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower.. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® C 9021 M POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with molybdenum disulphide modifiedInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® C 9021 XAP² ™ POM
(Unverified Data**) POM copolymerLow EmissionInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | ASTM D1525 |
Kolon KOCETAL® K300EW Standard Grade Acetal Resin General injection molding grade, toughness is slightly improved. Applications: General injection molding products.Information provided by API-Kolon. |
|||
Melting Point | 166 °C | 331 °F | ASTM D1525 |
Kolon KOCETAL® K300HRD Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Melting Point | 166 °C | 331 °F | ASTM D1525 |
Kolon KOCETAL® UR304 Toughened Grade Acetal Resin TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon. |
|||
Melting Point | 166 °C | 331 °F | |
Borealis Borpact™ BC914TF Polypropylene Copolymer Borpact™ BC914TF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. This grade is especially developed for the manufacturing of unoriented f.. |
|||
Melting Point | 166 °C | 331 °F | ISO 3146 |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 901 VT POM Copolymer unreinforced, antistatic POMInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 904 GB POM Copolymer, 20% glass bead reinforced POM-GB20Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 - 186 °C | 331 - 367 °F | |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Melting Point | 166 °C | 331 °F | DIN 53765 |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Melting Point | 166 °C | 331 °F | DIN 53765 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® LX90 POM, Unfilled Preliminary Data SheetInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® S 9243 XAP² ™ LS POM, Impact Modified POM copolymer, modifiedInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® SXT90Z-01 XAP POM, Impact Modified Hostaform« acetal copolymer grade SXT90Z-01 XAP is UV stabilized, impact modified material available in a range of colors for automotive interior applications plus meets the typical low emission re.. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Celstran® PP-GF40-0414 P7/10 PP, 40% Glass Reinforced Material code according to ISO 1043-1: PPInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® C 27021 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® C 9021 M XAP²™ POM, Tribological POM copolymerInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | DSC, 10 K/min, Molding compound; ISO 3146, method C1b |
Celanese Hostaform® C 13021 RM Acetal Copolymer Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advant.. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® C 9021 M XAP2® POM Description: Injection molding type, modified with molybdenum disulphide; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to ther.. |
|||
Melting Point | 166 °C | 331 °F | DSC, 10 K/min, Molding compound; ISO 3146, method C1b |
Celanese Hostaform® S 27072 GV 1/10 Elastomer Modified Acetal Copolymer with 10% Glass Fiber Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advant.. |
|||
Melting Point | 166 °C | 331 °F | ISO 11357-1,-2,-3 |
Celanese Hostaform® S 9244 XAP2 ™ POM, Impact Modified POM copolymer, modifiedInformation provided by Celanese Corporation. |
|||
Melting Point | 166 °C | 331 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement.. |
|||
Melting Point | 166 °C | 331 °F | DSC, 10 K/m; ISO 3146 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |
|||
Melting Point | 166 °C | 331 °F | ASTM D789 |
Chem Polymer Formax 630 Acetal, High Flow A 30 melt flow index copolymer acetal for use in products requiring extreme demands on processing characteristics but only moderate demands on mechanical performance.Data provided by the manufacture.. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® S 27072 WS 10/1570 POM, Impact Modified
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POM-HIEasy flowing, elastomer-containing injection molding grade; black; weathering resistantInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Celstran® PP-GF30-0403 P10/10 PP, 30% Glass Reinforced Material code according to ISO 1043-1: PPInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® C 9021 GV3/30 POM, 30% Glass Reinforced Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Hostaform® MT8R02 POM, Medical Technology Hostaform« acetal copolymer grade MT8R02 is a special grade developed for medical industry applications containing low residual monomers. Hostaform« MT8R02 is an improved wear performance grade t.. |