Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
Palm Labs Adhesives TURBO-LOCK SERIES 14 Anaerobic Thread Locking Compound TURBO-LOCK 14 SERIES is a fast curing, high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water, gases, oi.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
DSM Biomedical PurSil® 10 Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® thermoplastic siliconepolyether-urethane (TSPU) is a novel copolymer that is strong, yet flexible with proven biocompatibility and biostability. Leveraging the benefits of both silicone ela.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
PolyOne Edgetek® AS-10GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ NL-15KV/000 Nylon 6/12, Aramid Fiber
(discontinued **) Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 LV Liquid Silicone Rubber - Low Volatile / High Tear This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LSR 3785/30 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
LG Chemical EM600 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Samyang Tramid® 910 PA66/PA6 Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.Applications:Automotive knob types, door handles and mirror housingsConnectorsCab.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
A. Schulman POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE DescriptionPOLYBLAK® Black 4692 is a premium black color concentrate containing 35% carbon black based in LLDPE. This carbon black masterbatch is designed to provide smooth extruded surfaces and e.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
E-Polymers SEPAZ® N3040IR Nanoclay 4% Impact Modified Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Specific Gravity | 1.11 - 1.15 g/cc | 1.11 - 1.15 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 3009 GK3 BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | uncured |
Atom Adhesives AA-BOND FDA2 Epoxy Adhesive AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and recei.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Conditioned Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Metallic Grey 80330/2 DescriptionPOLYBATCH® Metallic Grey 80330/2 is a metallic grey color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
PolyOne Edgetek® AS-10GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |