Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 154 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Thickness 3900 microns
154 mil
Sheet; Internal
Azdel Plus R300-B01 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Thickness 3900 microns
154 mil
Sheet; Internal
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co..
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Thickness 3900 microns
154 mil
AZDEL Test
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..