Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.00 GPa | 580 ksi | |
Plastcom SLOVAMID 6 T 10 PA6, mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYform POM C M90 GF10 Polyoxymethylene Information provided by Polykemi AB |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**) Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a.. |
|||
Flexural Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Flexural Modulus | 4.00 - 7.10 GPa | 580 - 1030 ksi | Average value: 5.52 GPa Grade Count:18 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Global NPP-130-C Glass/Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 4.00 - 4.50 GPa | 580 - 653 ksi | ASTM D790 |
Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Techmer ES HiFill® PEEK HF Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ISO 178 |
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant Impact modified, 13% glass fiber reinforced, heat resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | D790 |
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant Applications: Lamp partsHome electric appliance partsFeatures: Fine appearanceHigh rigidityImpact resistantInformation provided by Toyobo. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Unitika M2350 PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM-D790 |
Polyram PlusTek PD300G4 Nylon 12, 20% Glass Fiber 20% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790, ISO 178 |
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber Characteristics: 10% glass fibre filled |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber Contains 10% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® 551GT20S PBT Resin Glass fiber and mineral filled, flame retardant, low warpage, superior electrical performance, surface glossInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
Ashley Polymers Ashlene® 925LMS-22G Nylon 12, 22% Glass Reinforced A 22% glass reinforced, Molybdenum disulfide filled, Nylon 12 resin for injection molding.Data provided by the manufacturer |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ISO Value |
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur.. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | ISO Value |
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen.. |
|||
Flexural Modulus | 4.00 GPa | 580 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |