Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Unannealed; ISO 75-2/A |
PolyOne OnForce™ LFT PP-60LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | |
Covestro Apec® DP 1-9359/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ASTM D648 |
Kostat 5000 TAB Spacer Tapes PET 5000 TAB Spacer Tapes, uniquely formulated and manufactured by KOSTAT, are made of various thermoplastic substrates with ICP (Inherently Conductive Polymer) coating technology. This class of materi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ASTM D648 |
Kostat ICP-STAT ICS-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ASTM D648 |
Kostat ICP-STAT ICD-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C @Thickness 6.40 mm |
316 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP VERTON MV005SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MV005SX0 is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Asia Pacific) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East) LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ISO 75-1, 2 |
Polyplastics Duracon® GH-20 Acetal Co-polymer (POM), GF 20% reinforced, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ASTM D648 |
Plenco 7523 Phenolic, Granular, Transfer Molded PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ISO 75-1,-2 |
Covestro Apec® FR1892 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ASTM D648 |
Diamond Polymers NYLON 6650HSL Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | ISO 75/2a |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 158 °C | 316 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |