Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.04 - 1.38 g/cc
0.0376 - 0.0500 lb/in³
Average value: 1.14 g/cc Grade Count:58
Water Absorption 1.60 - 10.0 %
1.60 - 10.0 %
Average value: 6.35 % Grade Count:15
Moisture Absorption at Equilibrium 2.70 - 3.00 %
2.70 - 3.00 %
Average value: 2.94 % Grade Count:10
Water Vapor Transmission 2.60 - 465 g/m²/day
0.167 - 29.9 g/100 in²/day
Average value: 143 g/m²/day Grade Count:19
Oxygen Transmission 1.05 - 40.3 cc-mm/m²-24hr-atm
2.67 - 102 cc-mil/100 in²-24hr-atm
Average value: 4.49 cc-mm/m²-24hr-atm Grade Count:7
Oxygen Transmission Rate 0.230 - 192 cc/m²/day
0.0148 - 12.4 cc/100 in²/day
Average value: 27.2 cc/m²/day Grade Count:20
Viscosity 3.15 - 85.0 cP
3.15 - 85.0 cP
Average value: 10.3 cP Grade Count:5
810000 - 2.74e+6 cP

@Temperature 260 - 260 °C
810000 - 2.74e+6 cP

@Temperature 500 - 500 °F
Average value: 1.26e+6 cP Grade Count:6
200000 - 5.00e+6 cP

@Temperature 240 - 280 °C
200000 - 5.00e+6 cP

@Temperature 464 - 536 °F
Average value: 1.26e+6 cP Grade Count:6
200000 - 5.00e+6 cP

@Shear Rate 0.100 - 1000 1/s
200000 - 5.00e+6 cP

@Shear Rate 0.100 - 1000 1/s
Average value: 1.26e+6 cP Grade Count:6
Viscosity Test 155 - 229 cm³/g
155 - 229 cm³/g
Average value: 200 cm³/g Grade Count:10
Thickness 10.2 - 59.0 microns
0.400 - 2.32 mil
Average value: 30.7 microns Grade Count:35
Linear Mold Shrinkage 0.0140 cm/cm
0.0140 in/in
Average value: 0.0140 cm/cm Grade Count:5
Linear Mold Shrinkage, Transverse 0.0140 cm/cm
0.0140 in/in
Average value: 0.0140 cm/cm Grade Count:4
Melt Flow 3.00 - 50.0 g/10 min
3.00 - 50.0 g/10 min
Average value: 17.4 g/10 min Grade Count:12
Surface Tension 36.0 - 56.0 dynes/cm
36.0 - 56.0 dynes/cm
Average value: 52.9 dynes/cm Grade Count:17
Mechanical Properties Metric English Comments
Ball Indentation Hardness 60.0 - 140 MPa
8700 - 20300 psi
Average value: 100 MPa Grade Count:4
Tensile Strength, Ultimate 48.0 - 112 MPa
6960 - 16200 psi
Average value: 86.3 MPa Grade Count:6
Film Tensile Strength at Yield, MD 31.0 - 51.0 MPa
4500 - 7400 psi
Average value: 36.8 MPa Grade Count:12
Film Tensile Strength at Yield, TD 37.2 - 82.7 MPa
5400 - 12000 psi
Average value: 65.6 MPa Grade Count:10
Tensile Strength, Yield 28.0 - 80.0 MPa
4060 - 11600 psi
Average value: 60.1 MPa Grade Count:26
Film Elongation at Break, MD 50.0 - 460 %
50.0 - 460 %
Average value: 210 % Grade Count:35
Film Elongation at Break, TD 55.0 - 480 %
55.0 - 480 %
Average value: 294 % Grade Count:21
Elongation at Break 3.50 - 400 %
3.50 - 400 %
Average value: 120 % Grade Count:27
Elongation at Yield 4.00 - 25.0 %
4.00 - 25.0 %
Average value: 13.3 % Grade Count:10
Modulus of Elasticity 0.100 - 3.30 GPa
14.5 - 479 ksi
Average value: 1.75 GPa Grade Count:25
Flexural Yield Strength 28.0 - 120 MPa
4060 - 17400 psi
Average value: 74.9 MPa Grade Count:14
Flexural Modulus 0.690 - 2.80 GPa
100 - 406 ksi
Average value: 2.22 GPa Grade Count:10
Secant Modulus 0.650 GPa
94.3 ksi
Average value: 0.650 GPa Grade Count:6
Secant Modulus, MD 0.285 - 4.69 GPa
41.3 - 680 ksi
Average value: 2.17 GPa Grade Count:22
Secant Modulus, TD 0.285 - 3.70 GPa
41.3 - 537 ksi
Average value: 2.17 GPa Grade Count:20
Izod Impact, Notched 0.450 - 10.7 J/cm
0.843 - 20.0 ft-lb/in
Average value: 3.69 J/cm Grade Count:4
Charpy Impact Unnotched 1000 J/cm²
4760 ft-lb/in²
Grade Count:12
5.50 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
26.2 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.50 J/cm² Grade Count:8
Charpy Impact, Notched 0.500 - 5.00 J/cm²
2.38 - 23.8 ft-lb/in²
Average value: 2.02 J/cm² Grade Count:14
0.500 - 0.500 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.500 J/cm² Grade Count:8
Coefficient of Friction 0.150 - 2.00
0.150 - 2.00
Average value: 0.587 Grade Count:29
Coefficient of Friction, Static 0.370 - 1.40
0.370 - 1.40
Average value: 0.998 Grade Count:10
Tear Strength Test 23.0 - 14000
23.0 - 14000
Average value: 1090 Grade Count:28
Elmendorf Tear Strength MD 56.0 g
56.0 g
Average value: 56.0 g Grade Count:6
Elmendorf Tear Strength, MD 0.394 - 4.21 g/micron
10.0 - 107 g/mil
Average value: 1.86 g/micron Grade Count:4
Elmendorf Tear Strength, TD 1.57 - 7.87 g/micron
40.0 - 200 g/mil
Average value: 4.74 g/micron Grade Count:4
Film Tensile Strength at Break, MD 32.0 - 379 MPa
4640 - 55000 psi
Average value: 184 MPa Grade Count:35
Film Tensile Strength at Break, TD 29.0 - 303 MPa
4210 - 44000 psi
Average value: 128 MPa Grade Count:21
Thermal Properties Metric English Comments
CTE, linear 80.0 - 100 µm/m-°C
44.4 - 55.6 µin/in-°F
Average value: 85.0 µm/m-°C Grade Count:14
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
Average value: 80.0 µm/m-°C Grade Count:8
Specific Heat Capacity 1.55 - 2.55 J/g-°C
0.370 - 0.609 BTU/lb-°F
Average value: 1.92 J/g-°C Grade Count:6
Melting Point 193 - 260 °C
379 - 500 °F
Average value: 220 °C Grade Count:30
Deflection Temperature at 0.46 MPa (66 psi) 51.0 - 161 °C
124 - 322 °F
Average value: 136 °C Grade Count:12
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 75.0 °C
122 - 167 °F
Average value: 54.9 °C Grade Count:17
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 - 1.00e+15 ohm-cm
1.00e+12 - 1.00e+15 ohm-cm
Average value: 2.00e+14 ohm-cm Grade Count:12
Surface Resistance 1.00e+13 - 1.00e+15 ohm
1.00e+13 - 1.00e+15 ohm
Average value: 2.57e+14 ohm Grade Count:12
Dielectric Constant 3.50 - 18.0
3.50 - 18.0
Average value: 7.35 Grade Count:8
Dielectric Strength 30.0 - 35.0 kV/mm
762 - 889 kV/in
Average value: 32.0 kV/mm Grade Count:12
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:12