Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 0.100 - 1.00e+12 ohm | 0.100 - 1.00e+12 ohm | Average value: 1.30e+10 ohm Grade Count:69 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Surface Resistance | 0.100 - 1.00e+15 ohm | 0.100 - 1.00e+15 ohm | Average value: 1.08e+14 ohm Grade Count:23 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |