Polymer Property : Surface Resistance = 1.30e+13 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance >= 1.30e+13 ohm
>= 1.30e+13 ohm
ASTM D257
Zircar Refractory Composites RS-201 Refractory Sheet
ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Surface Resistance >= 1.30e+13 ohm
>= 1.30e+13 ohm
ASTM D257
Zircar Refractory Composites RS-202 Refractory Sheet
ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Surface Resistance 1.30e+13 ohm
1.30e+13 ohm
Arkema Group Orgalloy® LT 4060IH Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (200 MPa), good ..
Surface Resistance 1.30e+13 - 1.00e+15 ohm
1.30e+13 - 1.00e+15 ohm
Average value: 8.03e+14 ohm Grade Count:5
Overview of materials for Nylon, Flexible Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri..