Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer RheTech Products
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
23/23°C; ASTM D792
Filler Content 0.00 %
0.00 %
ASTM D5630
Linear Mold Shrinkage 0.0131 cm/cm
0.0131 in/in
ASTM D955
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength at Break 25.5 MPa
3700 psi
2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.801 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
Front Barrel Temperature 199 - 227 °C
390 - 440 °F
Nozzle Temperature 204 - 216 °C
400 - 420 °F
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
Dry Time 1 - 2 hour
1 - 2 hour
Moisture Content <= 0.050 %
<= 0.050 %
Recommended
Injection Pressure 2.76 - 10.3 MPa
400 - 1500 psi
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Users viewing this material also viewed the following: