Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hold Pressure = 300 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 6.89 MPa
300 - 1000 psi
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey
Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 6.89 MPa
300 - 1000 psi
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 6.89 MPa
300 - 1000 psi
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment
Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP521-501UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 149B Shale
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP522-390 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, AYCA Medium Prairie
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White
Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural
Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products..
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black
Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black
Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP531-01UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: IP structural componentsAir ducts - distributionA/B/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved