Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 380 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 193 - 232 °C
380 - 450 °F
Multibase Multi-Pro® 2510 XGW Polypropylene
Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal
Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P100-00 Polypropylene, Natural
Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black
Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P251-01 Polypropylene Copolymer, Black
Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P254-01 Polypropylene Copolymer, Black
Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black
Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 193 - 210 °C
380 - 410 °F
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer
SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP...
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer
SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5..
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
CTC X-PRO CTC PP 2025 Polypropylene Impact Copolymer
X-PRO PP 2025 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
CTC X-PRO CTC PP 2040 Polypropylene Copolymer
X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
CTC X-PRO CTC PP 3020 Polypropylene Copolymer
X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
CTC X-PRO PP 2050 Polypropylene Copolymer
X-PRO PP 2050 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Middle Barrel Temperature 193 - 232 °C
380 - 450 °F
Multibase Multi-Pro® 4007 XGS Polypropylene
Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase
Copyright © lookpolymers.com All Rights Reserved