Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: 833 ppm Thermal Stabilizer: YesApplications: Agricultural FilmCo-Extrusion FilmsFoamsForm Fill and Seal PackagingFreezer FilmLamination FilmPoultry BagRice BagsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ExxonMobil method
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Antiblock Level 1500 ppm
1500 ppm
Slip Level 833 ppm
833 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 430 %
430 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Elmendorf Tear Strength MD 100 g
100 g
ASTM D1922
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
Dart Drop Test 280 g
0.617 lb
ASTM D1709A
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
Film Tensile Strength at Break, TD 26.2 MPa
3800 psi
ASTM D882
1% Secant Modulus, MD 159 MPa
23000 psi
ASTM D882
1% Secant Modulus, TD 179 MPa
26000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003
Gloss 52 %
52 %
45°; ASTM D2457
Users viewing this material also viewed the following: