| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
|
Multibase Multi-Pro® 3014 XUGW Polypropylene
Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase
|
|||
| Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
|
Multibase Multi-Pro® 3018 XUG Polypropylene
Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey
Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products P104-00 Polypropylene, Natural
Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products P107-00 Polypropylene Homopolymer, Natural
Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products P250-00 Polypropylene Copolymer, Natural
Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products P254-00 Polypropylene Copolymer, Natural
Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
|
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
|
|||
| Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
|
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 243 °C | 379 - 469 °F | |
|
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over..
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
|
|||
| Middle Barrel Temperature | 193 - 210 °C | 380 - 410 °F | |
|
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer
SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5..
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer
X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer
X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC).
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
CTC X-PRO CTC PP 2040 Polypropylene Copolymer
X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
CTC X-PRO PP 2021 Polypropylene Impact Copolymer
X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC).
|
|||
| Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
|
Multibase Multi-Pro® 4007 XGS Polypropylene
Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase
|
|||
| Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
|
LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact
V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc.
|
|||