| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 204 °C | 400 °F | |
|
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black
Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 210 °C | 400 - 410 °F | |
|
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey
Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral
Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT2400-648UV Thermoplastic Polyolefin, UV Stabilized, 848 Black
Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P107-00 Polypropylene Homopolymer, Natural
Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P251-00 Polypropylene Copolymer, Natural
Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P254-01 Polypropylene Copolymer, Black
Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 221 °C | 400 - 430 °F | |
|
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer
SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP...
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC SunPro® SP 200 P4058 Polypropylene Copolymer
SunPro® SP 200 P 4058 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: Chrysl..
|
|||
| Nozzle Temperature | 204 - 221 °C | 400 - 430 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t..
|
|||
| Nozzle Temperature | 204 - 221 °C | 400 - 430 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t..
|
|||
| Nozzle Temperature | 204 - 221 °C | 400 - 430 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,..
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | Average value: 210 °C Grade Count:3 |
|
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..
|
|||