Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 182 - 227 °C | 360 - 441 °F | |
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE) Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |